2014-3-6A representative feed sample of White Silica Sand was wet-sieved in order to recover the desired fractions for glass making. BIS specification shows that 600, 300 m fraction A should not be more than 50 and 300, 125 m fraction B should be 50 minimum. The mass percentage of A and B is found to be 29.9 and 70.1 ratio 13.34 which satisfies the size specifications for.